Allvac® Astroloy Nickel Superalloy, Heat Treatment: 1163°C (2125°F) + Age
Subcategory: Superalloy; Nickel Base
Key Words: UNS N13017; AMS 5851, 5852, 5882, Allvac, an Allegheny Teledyne Company
Material Notes: Nickel content calculated as remainder. Data provided by Allvac. Applications: Discs, rings, bolts for gas turbines.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|
| Property Data |