Allvac® 35N Nickel Superalloy, Heat Treatment: 1052°C (1925°F) + Age
Subcategory: Superalloy; Nickel Base; Cobalt Base
Key Words: UNS R30035; AMS 5758. ASTM F 562; Cobalt Alloys; Allvac, an Allegheny Teledyne Company
Material Notes: Cobalt content calculated as remainder. Data provided by Allvac. Applications: Aircraft fasteners. Line wire for down-hole instrumentation. Biomedical devices, high fatigue strength applications.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|