Allvac® 70, Ti CP-4 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Subcategory: Titanium Alloy; Nonferrous Metal; Unalloyed/Modified Titanium
Key Words: UNS R50700; AMS 4901, 4921; MIL-T-9046, -9047. ASTM F 67, Titanium Grade 4; ASTM B 265, 337, 338, 348, 381; Allvac, an Allegheny Teledyne Company
Material Notes: Titanium content calculated as remainder. Data provided by Allvac. Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|