Allvac® 3-2.5 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Near Alpha Titanium Alloy
Key Words: UNS R56320; AMS 4943, 4944; MIL-T-9046, -9047. ASTM B 265, 337, 338, 348, 381, Ti-3Al-2.5V; Half 6-4; Ti-3-2.5; Allvac, an Allegheny Teledyne Company
Material Notes: Titanium content calculated as remainder. Data provided by Allvac. Applications: Excellent cold formability, 20-50% higher tensile properties than CP titanium grades. Primarily used in aircraft hydraulic systems.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|