Allvac® 6-4ELI Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Beta Titanium Alloy
Key Words: UNS R56401; AMS 4907, 4930, 4931. MIL-T-9046, -9047, -81556; ASTM F 136, Ti-6Al-4V; Ti-6-4; Allvac, an Allegheny Teledyne Company
Material Notes: Titanium content calculated as remainder. Data provided by Allvac. Applications: Applications requiring excellent fracture toughness and fatigue strength; aircraft, structural components, biomedical.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|