Allvac® 8-1-1 Titanium Alloy, Heat Treatment: 982°C (1800°F) + Age
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Near Alpha Titanium Alloy
Key Words: UNS R54810; AMS 4915, 4933, 4972. MIL-T-81556, -83142, Ti-8Al-1Mo-1V; Ti-811; Allvac, an Allegheny Teledyne Company
Material Notes: Titanium content calculated as remainder. Data provided by Allvac. Applications: Fan & compressor blades, discs, spacers, seals, rings. Excellent creep resistance. Standard, rotor/premium grades.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|