Allvac® 6-2-4-6 Titanium Alloy, Heat Treatment: 885°C (1625°F) + Age
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Beta Titanium Alloy
Key Words: UNS R56260; AMS 4981. MIL-T-9047, -83142, Ti-6Al-2Sn-4Zr-6Mo; Ti-6246; Allvac, an Allegheny Teledyne Company
Material Notes: Titanium content calculated as remainder. Data provided by Allvac. Applications: Intermediate-temperature jet engine applications. Blades, discs, spacers, seals. Standard, rotor/premium grades.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|