VascoMax® C-350 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age
Subcategory: Maraging Steel; Metal
Key Words: Allvac, an Allegheny Teledyne Company; Maraging Steel, PWA 1091. PDS 10705Z2.
Material Notes: Iron content calculated as remainder. Data provided by Allvac. Applications: Missile components. Tooling. Spring wire for valve springs in high-performance internal combustion engines.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|