Vasco® 13-8Mo Precipitation Hardening Steel, Heat Treatment: 927°C (1700°F) + Age
Subcategory: Stainless Steel; Precipitation Hardening Stainless; Metal
Key Words: Allvac, an Allegheny Teledyne Company; Maraging Steel, UNS S13800; AMS 5629. DMS 2100; ASTM A 564; PH 13-8 Mo, 13-8Mo, 13-8PH, 13-8 PH, 13/8 Mo, 13/8Mo, 13/8PH, 13/8 PH
Material Notes: Iron content calculated as remainder. Data provided by Allvac. Applications: Airframe structurals, missile components, valve parts, fasteners, chemical process equipment.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|