Vasco® 15-5 Precipitation Hardening Steel, Heat Treatment: 1038°C (1900°F) + Age
Subcategory: Stainless Steel; Precipitation Hardening Stainless; Metal
Key Words: Allvac, an Allegheny Teledyne Company, UNS S15500; AMS 5659. ASTM A564, ASTM A564M, ASTM A705, ASTM A705M, 15-5PH, 15-5 PH, 15/5PH, 15/5 PH, Precipitation Hardening
Material Notes: Iron content calculated as remainder. Data provided by Allvac. Applications: Aircraft and missile fittings, fasteners, gears. Turbine and pump blades, shafts.