Vasco® 316-L Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Key Words: Allvac, an Allegheny Teledyne Company, UNS S31603; AMS 5507, 5653, 5648, 5649; AISI 316L, ASTM A167, A182, A213, F138, biomaterials, biomedical implants
Material Notes: Iron content calculated as remainder. Data provided by Allvac. Applications: Jet engine components, exhaust manifold heat exchangers, chemical process equipment, semiconductor systems.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|
| Property Data |