Vasco® Greek Ascoloy Specialty Steel, Heat Treatment: 871°C (1600°F) + Age
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal
Key Words: Allvac, an Allegheny Teledyne Company, UNS S41800; AMS 5508, 5616. MTS 1150
Material Notes: Iron content calculated as remainder. Data provided by Allvac. Applications: Compressor blades, vanes, disks, shafts, wheels, fasteners, gas turbine and jet engine components.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|
| Property Data |