Nickelvac® H-46 Specialty Steel, Heat Treatment: 1149°C (2100°F) Anneal
Subcategory: Stainless Steel; Metal
Key Words: Allvac, an Allegheny Teledyne Company, PWA 1091. PDS 10705Z2.
Material Notes: Iron content calculated as remainder. Data provided by Allvac. Applications: Structural components for land-based turbine engines. Rings and structurals in jet engines.