Nickelvac® 400 UNS N04400 Nickel Superalloy
Subcategory: Superalloy; Nickel Alloy; Nonferrous Metal; Nickel Base
Key Words: AMS 4675, 4730. ASTM B 127, B 164, B 564
Material Notes: Copper content calculated as remainder. Nickel-Copper solid solution alloy. Uses: Equipment for mineral acids, brines, alkalis, offshore engineering, marine applications. Property values are for samples in the metallurgical condition: 1650°F anneal. Information provided by Allvac, An Allegheny Teledyne Company.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|