Nickelvac® K-500 UNS N05500 Nickel Superalloy
Subcategory: Superalloy; Nickel Alloy; Nonferrous Metal; Nickel Base
Key Words: AMS 467. ASTM F 467, F 468.
Material Notes: Copper content calculated as remainder. Uses: Pump and drive shafts, impellers, valve components, springs, fasteners, oil well packers, subsurface safety valves. Property values are for samples in the metallurgical condition: 1600°F anneal + water quench + age. Information provided by Allvac, An Allegheny Teledyne Company.
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|