Allvac® Allcorr® UNS N06110 Nickel Superalloy
Subcategory: Superalloy; Nickel Alloy; Nonferrous Metal; Nickel Base
Key Words: ASTM B 564, B 755, B 756, B757, B 758, B 759.
Material Notes: Nickel content calculated as remainder. Uses: Equipment for deep sour gas wells, flue gas desulfurization, chemical and hydrocarbon processing, and pulp and paper. Property values are for samples in the metallurgical condition: 2050°F anneal. Information provided by Allvac, An Allegheny Teledyne Company.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|