Nickelvac® C 22 UNS N06022 Nickel Superalloy
Subcategory: Superalloy; Nickel Alloy; Nonferrous Metal; Nickel Base
Key Words: ASTM B 564, B 574, B 575, B 619, B 622, B 626.
Material Notes: Nickel content calculated as remainder. Uses: Pressure vessels, pumps, valves, HX tubing and piping for the CPI and HPI. Trays, flanges, fasteners, wire, screens. Property values are for samples in the metallurgical condition: 2050°F age. Information provided by Allvac, An Allegheny Teledyne Company.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|