Allvac® 718-OP® UNS N07718 Nickel Superalloy
Subcategory: Superalloy; Nickel Alloy; Nonferrous Metal; Nickel Base
Key Words: AMS 5662, 5663, 5664. MIL-N-24469, RDT M2-18T, ASTM B 637.
Material Notes: Iron content calculated as remainder. Uses: Turbines and engines, fasteners, sub-surface safety valves, hot extrusion tooling, nuclear reactors. Property values are for samples in the metallurgical condition: 1800°F age. Information provided by Allvac, An Allegheny Teledyne Company.
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|