Nickelvac® 606 Nickel Superalloy
Subcategory: Superalloy; Nickel Alloy; Nonferrous Metal; Nickel Base
Key Words: AWS Class ERNiCr-3. MIL-E-21562 type RN 82, EN 82.
Material Notes: Nominal nickel content reported herein also includes cobalt. Uses: Weld wire, woven wire mesh belts. Property values are for samples in the metallurgical condition: 2000°F anneal + water quench. Information provided by Allvac, An Allegheny Teledyne Company.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|
| Property Data |