Nickelvac® 825 UNS N08825 Nickel Superalloy
Subcategory: Superalloy; Iron Base
Key Words: ASTM B 163, B 423, B 424, B 425, B 704.
Material Notes: Iron content calculated as remainder. Uses: Downhole tubulars for deep, corrosive wells. Pollution control, scrubber, and radwaste systems. CPI process piping systems. Property values are for samples in the metallurgical condition: 2100°C anneal. Information provided by Allvac, An Allegheny Teledyne Company.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|