Nickelvac® TJA-1537™ UNS R31537 & UNS R31538 Nickel Superalloy
Subcategory: Superalloy; Nonferrous Metal; Cobalt Alloy
Key Words: ASTM F 1537; ISO 5832-12.
Material Notes: Cobalt content calculated as remainder. Cobalt-base alloy for machined and forged medical and surgical devices requiring high fatigue strength; total joint replacement. Property values are for samples in the metallurgical condition: Warm worked. Information provided by Allvac, An Allegheny Teledyne Company.
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|