Allvac® Grade 15-3-3-3 UNS R58153 Titanium Alloy
Subcategory: Titanium Alloy; Nonferrous Metal; Beta Titanium Alloy
Key Words: AMS 4914.
Material Notes: Titanium content calculated as remainder. Metastable beta titanium alloy. Uses: Industrial and aerospace components, pressure vessels, fittings, tubing, fasteners. Property values are for samples in the metallurgical condition: 1600°F anneal + water quench + age. Information provided by Allvac, An Allegheny Teledyne Company.
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|