Nickelvac® XM-19 UNS S20910 Specialty Steel
Subcategory: Stainless Steel; Metal
Key Words: AMS 5764; ASTM A 182, A 184, A 193, A 194, A 240, A 249, A 269, A 312, A 336, F 1314.
Material Notes: Iron content calculated as remainder. Uses: Chemical processing equipment, high-strength pump shafts, surgical implants, intermedullary nails, plates, screws, wires. Property values are for samples in the metallurgical condition: 1900°F 1 hr. + water quench. Information provided by Allvac, An Allegheny Teledyne Company.