Nickelvac® 304 L UNS S30403 Specialty Steel
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Key Words: aisi304, aisi 304, AMS 5511, 5647; AISI 304 L. ASTM A 167, A 182, A 213, A 240, SUS304, SS304
Material Notes: Iron content calculated as remainder. Widely used stainless steel for corrosion resistant application. CPI HX and vessels, tubing, wire, medical and dental devices. Property values are for samples in the metallurgical condition: 1900°F anneal. Information provided by Allvac, An Allegheny Teledyne Company.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|