Allvac® 9310 UNS G93106, UNS H93100 Specialty Steel
Subcategory: Low Alloy Steel; AISI 9000 Series Steel; Low Carbon Steel; Metal
Key Words: AISI 9310; AMS 6260, 6265, 6267. ASTM A 29, A 331, A519, A 646.
Material Notes: Iron content calculated as remainder. Uses: Automotive applications, structural components, gears, rods, heat-treatable shafts. Property values are for samples in the metallurgical condition: 1630°F normalized. Information provided by Allvac, An Allegheny Teledyne Company.