AL 6XN® UNS N08367 Specialty Steel
Subcategory: Stainless Steel; Metal
Key Words: AL6XN; ASTM B 472, B 564, B 688, B 690, B 691.
Material Notes: Iron content calculated as remainder. Uses: Process equipment, flue-gas scrubber systems, multi-effect evaporators for brines, seawater, pulp & paper liquors. Property values are for samples in the metallurgical condition: 2050°F anneal. Information provided by Allvac, An Allegheny Teledyne Company.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|