AMPCO METAL AMPCO® 8 Aluminum Bronze, Extruded and Drawn Rods, ≤ 12.7 mm.
Subcategory: Copper Alloy; Nonferrous Metal; Bronze
Close Analogs: Composition Notes: Copper content calculated from balance.
Material Notes: AMPCO 8 extruded has a high tensile strength and a good yield along with an inherent toughness and ductility not usually found in a single alpha phase aluminum bronze. During the extrusion process the metal is hot worked resulting in a compact grain structure free of inclusions or other defects and improved physical properties.Applications: AMPCO 8 is used whenever good resistance to corrosion, erosion, abrasion and cavitation-pitting is essential. AMPCO 8 is ideally suited for pipes, tubes, joints and other pieces used in the process, marine or other similar industries. The extreme hardness of this alloy makes it an ideal bolting material. AMPCO 8 has excellent bearing characteristics. It is used for bushings, bearings, wear strips and in similar applications where hardness and ductility are essential for uninterrupted operations.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Compressive Yield Strength
- Compressive Strength
- Charpy Impact
- Izod Impact
- Shear Strength
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|