AMPCO METAL AMPCO® 18 Aluminum Bronze, Extruded and Drawn Rods, 12.7 - 25.4 mm.
Subcategory: Copper Alloy; Nonferrous Metal; Bronze
Close Analogs: Composition Notes: Copper content calculated from balance.
Material Notes: Compact grain structure and high physical properties result from proper phase distribution and hot working of AMPCO 18 during the extrusion process. These qualities enable this alloy to perform successfully in an extremely wide range of difficult applications. It is an excellent bearing material characterized by good resistance to wear and fatigue.Applications: AMPCO 18 rod is produced with a good surface finish to commercial tolerances and can be used economically for volume-production applications. AMPCO 18 is ideally suited where high strength and hardness combined with wear and fatigue resistance are required. Some of the more common applications of this alloy are bushings, bearings, gears, worm wheels, valve seats and guides, hydraulic valve parts, pump rods, guide pin bushings, gibs and slides, etc.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Compressive Yield Strength
- Compressive Strength
- Charpy Impact
- Izod Impact
- Fatigue Strength
- Shear Strength
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|