AMPCO METAL AMPCO® 18.136 Aluminum Bronze, Centrifugal
Subcategory: Copper Alloy; Nonferrous Metal; Bronze
Close Analogs: Composition Notes: Copper content calculated from balance.
Material Notes: AMPCO 18.136 is a variation of AMPCO 18 specifically heat-treated to increase the impact resistance by 40 % (see Charpy values) and the elastic limit in compression by 10 % without affecting the tensile strength of the alloy.Applications: This AMPCO 18.136 has been tailor-made for steel mill applications as slippers and screw-down nuts and for similar applications where an extreme wear pressure is combined with important impact loading.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Compressive Yield Strength
- Compressive Strength
- Charpy Impact
- Izod Impact
- Fatigue Strength
- Shear Strength
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|