AMPCO METAL AMPCO® 22 Aluminum Bronze, Extruded Bar
Subcategory: Copper Alloy; Nonferrous Metal; Bronze
Close Analogs: Composition Notes: Copper content calculated from balance.
Material Notes: AMPCO 22 is a duplex structure alloy of approx. 50 % of each phase - gamma 2 and beta. It is remarkable because of its hardness, its excellent compression and wear resistance and by its sliding properties. As the elongation of the material is very low, thin sections should be avoided and the material should be well backed up.Applications: The field of service of AMPCO 22, with few exceptions, is limited to forming and/or drawing stainless steel, especially when runs are long or gauge is heavy and it is essential that tolerances be maintained.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Compressive Yield Strength
- Compressive Strength
- Charpy Impact
- Izod Impact
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|