AMPCO METAL AMPCOLOY® 95 Cobalt-Copper Alloy, Extrusion, ≤ 50.8 mm.
Subcategory: Copper Alloy; Nonferrous Metal
Close Analogs: Composition Notes: Copper content calculated from balance.
Key Words: CDA C17500; RWMA Class 3; ISO NFA 82100; EN CW 103C Typ A3/1; DIN 17666 W. Nr. 2.1285; AFNOR UK2Be
Material Notes:
Applications: AMPCOLOY 95 finds its own applications due to its slightly higher mechanical properties. AMPCOLOY 95 is principally used for spot welding electrodes, electrodes for mesh welding, electrode holders and seam welding discs for stainless steel, Monel and nickel alloys, flash welding dies, plunger tips in aluminum high pressure die casting machines and parts for injection moulding of plastic wherever a high thermal conductivity is desirable.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|