AMPCO METAL AMPCOLOY® 95 Cobalt-Copper Alloy, Extrusion, >50.8 mm.

 

Subcategory: Copper Alloy; Nonferrous Metal

Close Analogs:

Composition Notes: Copper content calculated from balance.

Key Words: CDA C17500; RWMA Class 3; ISO NFA 82100; EN CW 103C Typ A3/1; DIN 17666 W. Nr. 2.1285; AFNOR UK2Be

Material Notes:

Applications: AMPCOLOY 95 finds its own applications due to its slightly higher mechanical properties. AMPCOLOY 95 is principally used for spot welding electrodes, electrodes for mesh welding, electrode holders and seam welding discs for stainless steel, Monel and nickel alloys, flash welding dies, plunger tips in aluminum high pressure die casting machines and parts for injection moulding of plastic wherever a high thermal conductivity is desirable.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Electrical Resistivity
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。