AMPCO METAL AMPCOLOY® 972 Chromium-Copper Alloy, Extruded and Drawn Rods, 10 - 25 mm.
Subcategory: Copper Alloy; Nonferrous Metal
Close Analogs: Composition Notes: Copper content calculated from balance.
Key Words: CDA C18150; CDA C18200; CDA C18400; RWMA Class2, CuCr1Zr; EN CW 106C; DIN 44759 A 2/2 17666 W.Nr. 2.1293; AFNOR UC1Zr
Material Notes: AMPCOLOY 972 is a precipitation hardening copper-base-alloy. In the heat treated condition, this alloy retains the mechanical properties together with a good ductility in the range of 300-500°C. High electrical conductivity and high mechanical properties are attributes of this versatile alloy.Applications: Resistance welding tips; Electrode caps for the automotive industry; Tong arms for welding robots; Electrode holders; Parts for energy engineering; Press parts
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|