AMPCO METAL AMPCOLOY® 30 Leaded Bronze, Centrifugally Cast
Subcategory: Copper Alloy; Nonferrous Metal; Bronze; Copper Casting Alloy
Key Words: CDA 93800; DIN 1716 CuPb15Sn 2.1182.04; DIN 1716 CuPb15Sn 2.1182.03; DIN 1716 CuPb15Sn 2.1182.01; AFNOR U Pb 15 E8
Material Notes: Copper Alloy with low friction properties. Resistant to sea water and sulfuric acid. Specific pressure up to 20 Mpa. Linear speed up to 12 m/sec.Applications: High speed medium load bearings where lubrication is not always guaranteed
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
|
|
|
|