AMPCO METAL AMPCOLOY® 35 Tin Bronze, Continuous Cast
Subcategory: Copper Alloy; Nonferrous Metal; Bronze; Copper Casting Alloy
Key Words: CDA C 93200; DIN 1705 CuSN7ZnPb 2.1090.04; DIN 1705 CuSN7ZnPb 2.1090.03; DIN 1705 CuSN7ZnPb 2.1090.01; AFNOR U-E 7 Z5 Pb4
Material Notes: Copper Alloy with specific pressure up to 40 Mpa and linear speed up to 7 m/sec.Applications: Axle-bearing and coupling rod bearings, plain bearing for general mechanical engineering applications; Medium stressed bearing pads and adjusting gibs; Normally and highly stressed plain bearing bushing using shafts of unhardened steels; When light edge loading is involved.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|