AMPCO METAL AMPCOLOY® 712 Tin Bronze, Centrifugally Cast
Subcategory: Copper Alloy; Nonferrous Metal; Bronze; Copper Casting Alloy
Key Words: CDA C 91700; DIN 1705 CuSn12Ni 2.1052.04; DIN 1705 CuSn12Ni 2.1052.03; DIN 1705 CuSn12Ni 2.1052.01
Material Notes: Alloy used primarily for its excellent mechanical and corrosion resistance. Specific pressure up to 60 Mpa. Linear speed up to 6 m/sec.Applications: Spindle screw; Pressure screw-nut; Gear wheel; Machine tool parts
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
|
|
|
|