AMPCO METAL CuAl10Ni5Fe4 Aluminum Bronze, Extruded Rod
Subcategory: Copper Alloy; Nonferrous Metal; Bronze
Close Analogs: Composition Notes: Copper content calculated from balance.
Key Words: CDA C63000; DIN 17665 CuAl10Ni5Fe4 2.0966; AFNOR CuAl9Ni5Fe3M1
Material Notes: Aluminum bronze extruded rodsApplications: Construction material with good strength properties, sea water resistant. Endless screws with high tooth pressures and good lubrication.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|