XADC-Armoloy® Diamond-Chrome Composite Coating
Subcategory: Metal Matrix Composite; Ceramic/Metallic Coating
Key Words: Chrome Plating
Material Notes: XADC-Armoloy® combines the Armoloy® TDC chromium coating with spherical diamond particulates. The XADC-Armoloy® coating enhances the durability of components used in a wide range of applications from plastic injection mold tooling to aerospace applications that require long life expectancy, extreme wear protection, low frictional characteristics and corrosion protection. XADC-Armoloy® will not fracture from the basis metal unless the metal substrate itself fractures or fatigues. The absolute, positive adhesion that is created with the special application of XADC-Armoloy® is a major benefit to its users. Applied at temperatures under 200°F (100°C) there are absolutely NO changes in the basis metals that the XADC-Armoloy® coating is applied to. Like Armoloy® TDC, XADC-Armoloy® will adhere and perform well on all major ferrous and nonferrous basis materials. Aluminum, magnesium, and titanium are not considered good substrates for coating with Armoloy processes. Information provided by Armoloy of Western Pennsylvania.
| Available Properties |
- Thickness
- Hardness, Rockwell C
- Coefficient of Friction
- Coefficient of Friction, Static
- Taber Abrasion, mg/1000 Cycles
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|