Assab Steels 88 Cold Work Steel
Subcategory: Tool Steel; Chrome-moly Steel; Cold Work Steel; Metal
Material Notes: ASSAB 88 (SLEIPNER) is a chromium-molybdenum-vanadium alloyed tool steel which is characterized by:- Good wear resistance
- Good chipping resistance
- High compressive strength
- High hardness (>60HRC) after high temperature tempering
- Good through-hardening properties
- Good stability in hardening
- Good resistance to tempering back
- Good WEDM properties
- Good machinability and grindability
- Good surface treatment properties
ASSAB 88 (SLEIPNER) is a general purpose steel for cold work tooling. ASSAB 88 (SLEIPNER) is recommended for medium run tooling applications. Examples: - Blanking and fine blanking
- Shearing
- Forming
- Coining
- Cold forging
- Cold extrusion
- Thread rolling
- Drawing and deep drawing
- Powder pressing
| Available Properties |
- Density
- Hardness, Rockwell C
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Compressive Yield Strength
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|