Assab Steels XW-5 Cold Work Steel
Subcategory: Tool Steel; Cold Work Steel; High Carbon Steel; Metal
Close Analogs: AISI D6, (AISI D3), W.-Nr. 1.2436
Material Notes: ASSAB XW-5 is a high-carbon, high chromium tool steel alloyed with tungsten, characterized by:- High wear resistance
- High compressive strength
- High surface hardness after hardening
- Good through-hardening properties
- Good stability in hardening
- Good resistance to tempering-back
Applications: - blanking and shearing tools for thin, hard materials
- long-run press tools
- forming tools
- molds for ceramics and abrasive plastics
| Available Properties |
- Density
- Hardness, Rockwell C
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Compressive Strength
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|