Assab Steels XW-10 Cold Work Steel
Subcategory: Tool Steel; Cold Work Steel; Metal
Close Analogs: A2
Material Notes: Good hardenability and wear resistance. Excellent size stability. For medium runs.Blanking, punching, piercing, cropping, shearing, trimming, clipping.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|