Assab Steels XW-42 Cold Work Steel
Subcategory: Tool Steel; Chrome-moly Steel; Cold Work Steel; High Carbon Steel; Metal
Close Analogs: AISI D2
Material Notes: XW-42 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:- High wear resistance
- High compressive strength
- High hardness after hardening
- Good through-hardening properties
- Excellent dimensional stability in hardening
- Good resistance to tempering-back.
XW-42 is used when cutting thicker, harder materials; when forming with tools subjected to bending stresses and where high impact loads are involved. XW-42 can be supplied in various finishes, including the hot-rolled, pre-machined and fine machined condition. XW-42 is a good choice for inserts in larger tools as well as deep drawing tools.
| Available Properties |
- Density
- Hardness, Rockwell C
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Compressive Strength
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|