Assab Steels VANADIS 4 Cold Work Steel
Subcategory: Tool Steel; Chrome-moly Steel; Cold Work Steel; Metal
Material Notes: VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:- High wear resistance
- High compressive strength
- Very good through-hardening properties
- Very good toughness
- Excellent dimensional stability after hardening and tempering
- Good resistance to tempering back
VANADIS 4 is especially suitable for applications where adhesive wear and/or chipping are the dominating problems, i.e. - with soft/adherent materials such as austenitic stainless steel, mild steel, copper, aluminum, etc. as work material
- with thicker work material
Examples:- blanking and forming
- Fine blanking
- Cold extrusion tooling
- Powder pressing
- Deep drawing
- Knives
| Available Properties |
- Density
- Hardness, Rockwell C
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Impact Test
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|