Assab Steels ASP 23 Cold Work Steel

 

Subcategory: Tool Steel; Chrome-moly Steel; Cold Work Steel; Metal

Close Analogs: AISI M3:2/W.-Nr. 1.3344

Material Notes:
ASP 23 is a chromium-molybdenum-tungsten-vanadium alloyed high speed steel which is characterized by:

  • High wear resistance (abrasive profile)
  • High compressive strength
  • Very good through-hardening properties
  • Good toughness
  • Very good dimensional stability on heat treatment
  • Very good temper resistance

ASP 23 is especially suitable for blanking and forming of thinner work materials where a mixed (abrasive-adhesive) or abrasive type of wear is encountered and where the risk for plastic deformation of the working surfaces of the tool is high, e.g:

  • Blanking of medium to high carbon steels
  • Blanking of harder materials such as hardened or cold-rolled strip steels
  • Plastics mold tooling subjected to abrasive wear condition
  • Plastics processing parts, e.g. feed screws, barrel liners, nozzles, screw tips, non-return check ring valves, pellitizer blades, granulator knives.

Available Properties
  • Density
  • Hardness, Rockwell C
  • Hardness, Vickers
  • Modulus of Elasticity
  • Modulus of Elasticity at Elevated Temperature
  • Flexural Strength
  • Flexural Yield Strength
  • Impact Test
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  • Total Deflection, mm
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。