Assab Steels ASP 23 Cold Work Steel
Subcategory: Tool Steel; Chrome-moly Steel; Cold Work Steel; Metal
Close Analogs: AISI M3:2/W.-Nr. 1.3344
Material Notes: ASP 23 is a chromium-molybdenum-tungsten-vanadium alloyed high speed steel which is characterized by:- High wear resistance (abrasive profile)
- High compressive strength
- Very good through-hardening properties
- Good toughness
- Very good dimensional stability on heat treatment
- Very good temper resistance
ASP 23 is especially suitable for blanking and forming of thinner work materials where a mixed (abrasive-adhesive) or abrasive type of wear is encountered and where the risk for plastic deformation of the working surfaces of the tool is high, e.g: - Blanking of medium to high carbon steels
- Blanking of harder materials such as hardened or cold-rolled strip steels
- Plastics mold tooling subjected to abrasive wear condition
- Plastics processing parts, e.g. feed screws, barrel liners, nozzles, screw tips, non-return check ring valves, pellitizer blades, granulator knives.
| Available Properties |
- Density
- Hardness, Rockwell C
- Hardness, Vickers
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Flexural Strength
- Flexural Yield Strength
- Impact Test
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Total Deflection, mm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|