Assab Steels ASP 30 Cold Work Steel
Subcategory: Tool Steel; Cobalt Alloy; Cold Work Steel; Metal
Close Analogs: W.-NR. 1.3207
Material Notes: ASP 30 is a W-Mo-v-Co alloyed PM high speed steel characterized by:- High wear resistance
- High compressive strength at high hardness
- Good through hardening properties
- Good toughness
- Good dimensional stability on heat treatment
- Very good temper resistance
- The combination of high wear resistance and unusually good compressive strength can be put to use in tooling for heavy forming operations.
| Available Properties |
- Density
- Hardness, Rockwell C
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Flexural Strength
- CTE, linear 20°C
- Specific Heat Capacity
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|