Assab Steels ASP 60 Cold Work Steel
Subcategory: Tool Steel; Cobalt Alloy; Cold Work Steel; Metal
Close Analogs: W.-Nr. 1.3241
Material Notes: ASP 60 is a W-Mo-V-Co alloyed PM high speed steel characterized by:- Highest wear resistance
- Maximum compressive strength
- Good through hardening properties
- Good toughness
- Good dimensional stability on heat treatment
- Very good temper resistance
| Available Properties |
- Density
- Hardness, Rockwell C
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Flexural Strength
- CTE, linear 20°C
- Specific Heat Capacity
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|