Assab Steel 8407 2M Hot Work Steel
Subcategory: Chrome-moly Steel; Hot Work Steel; Metal
Close Analogs: AISI H13, W.-Nr. 1.2344
Material Notes: ASSAB 8407 is a chromium-molybdenum-vanadium-alloyed steel which is characterized by: - Good resistance to abrasion at both low and high temperatures.
- High level of toughness and ductility
- Uniform and high level of machinability and polishability
- Good high-temperature strength and resistance to thermal fatigue.
- Excellent through-hardening properties
- Very limited distortion during hardening.
Applications: Tools for Extrusion: Dies, backers, die holders, liners, dummy blocks, stems. Plastic molding applications: Injection molding of thermoplastics: long production runs. Molding of parts in thermosetting plastic with finish requirements.
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Impact Test
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|