Assab Steel 7210M Machinery Steel
Subcategory: Alloy Steel
Close Analogs: AISI /SAE 3115, DIN 15CrNi6, BS 637A16 (EN 352), AFNOR 16Nc6, JIS SNC21, SS 2511
Material Notes: ASSAB 7210M is an alloyed case hardening steel with high core strength.Applications: ASSAB 7210M is used for applications requiring a hard, wear resistant surface and a tough core, such as transmission components for the automotive industry. ASSAB 7210M is used for complicated parts, subject to strict demands on dimensional stability, core hardness and toughness.
| Available Properties |
- Hardness, Brinell
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Impact Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|