Assab Steel 760 Machinery Steel
Subcategory: Carbon Steel; Metal
Close Analogs: AISI 1148, JIS S50C
Material Notes: ASSAB 760 is an easily machinable carbon steel characterized by:- Good machinability
- Good mechanical strength
ASSAB 760 is primarily intended to be used in the as-delivered condition. It is only to be heat treated for special applications. Applications: Applications include: punch holders, die holders, guide plates, backing plates, jigs, fixtures, simple bending dies, simple structural components
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|